Examples

Drill pipes

Application, field
Material
Bonding dimensions

φ130.2×t18

Conventional technique

Merits of Adopting Izumi Equipment

Conventional technology: flash butt welding

Issues to be resolved

Flash butt welding
- Low bonding strength, use not possible for long parts
- Excavation depth limit of 2,000 m

Adoption merits

- Improved bonding strength with pressure welding
- Excavation possible to depth of 12,000 m

Applicable Model

Examples of Other Fields / Merits

Inflators
Inflators

SPFC×SPFC

Gate ball stick heads
Gate ball stick heads

TB35×A6063×TB35

Axle shafts
Axle shafts

S45C×S45C×SCM435

Copy rollers
Copy rollers

S15C×STKM13B×S15C

Click here for list of examples

Friction welding materials

Stable, complete joints are realized, even when combining dissimilar metals or nonferrous metals.

Inquiries

Please feel free to contact us for product information, technical information, or for support.