Examples

Torque rods

Application, field
Material
Bonding dimensions

φ45×t5

Conventional technique

Merits of Adopting Izumi Equipment

Conventional technology: flash butt welding

Issues to be resolved

Flash butt welding
- Welding strength defects
- High forging cost
- Spatter adhesion

Adoption merits

- Improved bonding strength, accuracy
- Reduced cost with adoption of simpler forging shape
- No spatter adhesion
- Improved bonded part appearance

Applicable Model

Examples of Other Fields / Merits

Box wrenches
Box wrenches

SCM435×SS400

City gas valves
City gas valves

C3771×C3771

Torque converter pump shells
Torque converter pump shells

SHP45×S15C

Turbine wheel shafts
Turbine wheel shafts

Inconel713C×SCM440H

Click here for list of examples

Friction welding materials

Stable, complete joints are realized, even when combining dissimilar metals or nonferrous metals.