Examples

Rolled bushings

Material
Bonding dimensions

φ90×t3.2

Conventional technique

Merits of Adopting Izumi Equipment

Conventional technology: monoblock part cutting

Issues to be resolved

Cutting from monoblock alloy casting
- High blank cost
- Trouble of poor wear resistance

Adoption merits

- Affixing of metal to SPC by machining workpieces separately
- Reduced blank cost
- Improved wear resistance

Applicable Model

Examples of Other Fields / Merits

Odd-shape reinforcing bar joints
Odd-shape reinforcing bar joints

S45C×SD345

Valve rods
Valve rods

C3771×C3771

Large switch parts
Large switch parts

C1100×C3771×C1100

Copy rollers
Copy rollers

S15C×STKM13B×S15C

Click here for list of examples

Friction welding materials

Stable, complete joints are realized, even when combining dissimilar metals or nonferrous metals.

Inquiries

Please feel free to contact us for product information, technical information, or for support.